We're commitment to offer you the competitive price ,remarkable products excellent, also as fast delivery for Steel Metal Pipe , Helical Seam Factory , X70 SSAW Line Pipe Exporters , Should you be fascinated in any of our products and services, remember to do not hesitate to make contact with us. We're ready to reply you inside of 24 several hours soon after receipt of one's ask for and also to develop mutual un-limited advantages and organization in around potential.
Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral Detail:

Chemical Composition of ASTM A234 WPB & WPC

Element

Content, %

ASTM A234 WPB

ASTM A234 WPC

Carbon [C]

≤0.30

≤0.35

Manganese [Mn]

0.29-1.06

0.29-1.06

Phosphorus [P]

≤0.050

≤0.050

Sulfur [S]

≤0.058

≤0.058

Silicon [Si]

≥0.10

≥0.10

Chromium [Cr]

≤0.40

≤0.40

Molybdenum [Mo]

≤0.15

≤0.15

Nickel [Ni]

≤0.40

≤0.40

Copper [Cu]

≤0.40

≤0.40

Vanadium [V]

≤0.08

≤0.08

*The Carbon Equivalent [C.E.=C+Mn/6+(Cr+Mo+V)/5+(Ni+Cu)/15] shall be no greater than 0.50 and shall be reported on MTC.

Mechanical Properties of ASTM A234 WPB & WPC

ASTM A234 Grades

Tensile Strength, min.

Yield Strength, min.

Elongation %, min

ksi

MPa

ksi

MPa

Longitudinal

Transverse

WPB

60

415

35

240

22

14

WPC

70

485

40

275

22

14

*1. WPB and WPC pipe fittings manufactured from plates shall have a minimum elongation of 17%.
*2. Unless required, hardness value doesn’t need to be reported.

Manufacture

The ASTM A234 carbon steel pipe fittings may be made from seamless pipes, welded pipes or plates by shaping operations of pressing, piercing, extruding, bending, fusion welding, machining, or by a combination of two or more these operations. All welds including welds in tubular products from which fittings are made shall be made in accordance with ASME Section IX. Post-weld heat treatment at 1100 to 1250°F[595 to 675°C] and radiographic examination shall be performed after the welding process.


Product detail pictures:

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures

Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral detail pictures


Related Product Guide:

We not only will try our greatest to supply outstanding services to every shopper, but also are ready to receive any suggestion offered by our buyers for Factory Cheap Hot Welding Thin Wall Tubing - ASTM A234 WPB & WPC pipe fittings including elbows, tee, reducers – Spiral , The product will supply to all over the world, such as: Singapore, Berlin, America, Being guided by customer demands, aiming at improving the efficiency and quality of customer service, we constantly improve products and provide more comprehensive services. We sincerely welcome friends to negotiate business and start cooperation with us. We hope to join hands with friends in different industries to create a brilliant future.
  • It is really lucky to meet such a good supplier, this is our most satisfied cooperation, I think we will work again!
    5 Stars By Eartha from Kyrgyzstan - 2018.02.21 12:14
    We have been cooperated with this company for many years, the company always ensure timely delivery ,good quality and correct number, we are good partners.
    5 Stars By Nydia from Latvia - 2018.11.02 11:11
    Write your message here and send it to us