We know that we only thrive if we will guarantee our combined cost competiveness and high-quality advantageous at the same time for Oil Pipe Line , Water Pipe Welding , The Pipe Line , We are now on the lookout ahead to even larger cooperation with abroad consumers dependant on mutual added benefits. When you are interested in almost any of our products, be sure to experience cost-free to make contact with us for more facts.
High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard – Spiral Detail:

Physical properties of epoxy powder materials

Specific gravity at 23℃: minimum 1.2 and maximum 1.8
Sieve analysis: maximum 2.0
Gel time at 200 ℃: less than 120s

Abrasive blast cleaning

Bare steel surfaces shall be abrasive blast-cleaned in accordance with SSPC-SP10/NACE No. 2 unless otherwise specified by the purchaser. The blast anchor pattern or profile depth shall be 1.5 mil to 4.0 mil(38 µm to 102 µm) measured in accordance with ASTM D4417.

Preheating

Pipe that has been cleaned shall be preheated at temperature less than 260℃, the heat source shall not contaminate the pipe surface.

Thickness

The coating powder shall be applied to the preheated pipe at a uniform cure-film thickness of not less than 12 mils(305μm) on the exterior or interior. The maximum thickness shall not exceed a nominal 16 mils(406μm) unless recommended by the manufacturer or specified by the pruchaser.

Optional epoxy performance testing

The purchaser may specify additional testing to establish epoxy performance. The following test procedures, all of which shall be performed on production pipe test rings, may be specified:
1. Cross-section porosity.
2. Interface porosity.
3. Thermal analysis (DSC).
4. Permanent strain (bendability).
5. Water soak.
6. Impact.
7. Cathodic disbondment test.


Product detail pictures:

High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard  – Spiral detail pictures

High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard  – Spiral detail pictures

High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard  – Spiral detail pictures


Related Product Guide:

We consistently execute our spirit of Innovation bringing progress, Highly-quality ensuring subsistence, Administration advertising and marketing gain, Credit history attracting buyers for High Quality For Pipe Welding Procedures - Fusion-Bonded Epoxy Coatings Awwa C213 Standard – Spiral , The product will supply to all over the world, such as: Malawi, Cairo, Czech Republic, As an experienced factory we also accept customized order and make it same as your picture or sample specifying specification and customer design packing. The main goal of the company is to live a satisfactory memory to all the customers, and establish a long term win-win business relationship. For more information, please contact us. And It is our great pleasure if you like to have a personally meeting in our office.
  • The supplier abide the theory of quality the basic, trust the first and management the advanced so that they can ensure a reliable product quality and stable customers.
    5 Stars By Dora from Grenada - 2017.04.18 16:45
    In our cooperated wholesalers, this company has the best quality and reasonable price, they are our first choice.
    5 Stars By Frances from Mumbai - 2018.12.11 14:13
    Write your message here and send it to us