Fast and good quotations, informed advisers to help you choose the correct product that suits all your needs, a short production time, responsible quality control and different services for paying and shipping affairs for Mild Steel Pipe Suppliers , Welding Thin Wall Tubing , Clutch Pipe Pilem , Customers' reward and fulfillment are usually our biggest objective. Please make contact with us. Give us a probability, provide you with a surprise.
High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral Detail:

Product Description

Cangzhou Spiral Steel Pipes Group Co., Ltd have 4 production lines of anticorrosion & thermal insulation to perform the 3LPE coating and FBE coating. The maximum outside diameter can be 2600mm.

The coatings are suitable for the protection of buried or submerged steel pipes at design temperatures of -40℃ to +80℃.

The present standard specifies requirements for coatings that are applied to spirally welded steel pipes and fittings used for the construction of pipelines for conveying liquids or gases.

Applying this standard ensures that the PE coating provides sufficient protection against the mechanical thermal and chemical loads occurring during operation, transport, storage and installation.

Extruded coatings comprise three layers: an epoxy resin primer, a PE adhesive and an extruded polyethylene outer layer. The epoxy resin primer is applied as a powder. The adhesive can be applied either as a powder or by extrusion. For extruded coatings a differentiation is made between sleeve extrusion and sheet extrusion. Sintered polyethylene coatings are single or multi-layer systems. The polyethylene powder is fused onto the pre-heated component until the desired coating thickness is reached.

Epoxy resin primer

The epoxy resin primer is to be applied in powder form. The minimum layer thickness is 60μm.

PE adhesive

The PE adhesive can be applied in powder form or extruded. The minimum layer thickness is 140μm. the peel strength requirements vary depending on whether the adhesive was applied as a powder or was extruded.

Polyethylene coating

The polyethylene coating is applied either by sintering or by sleeve or sheet extrusion. The coating is to be cooled after application to avoid unwanted deformation during transport. Depending on the nominal size, there are different minimum values for the normal total coating thickness. In the case of increased mechanical loads the minimu layer thickess shall be increased by 0.7mm. minimum layer thickness are given in table 3 below.

product-description1


Product detail pictures:

High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral detail pictures

High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral detail pictures

High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral detail pictures


Related Product Guide:

Our target should be to consolidate and improve the high-quality and repair of current goods, in the meantime regularly produce new solutions to meet unique customers' needs for High Quality For Pipe Welding Procedures - Outside 3LPE coating DIN 30670 inside FBE coating – Spiral , The product will supply to all over the world, such as: Palestine, Uganda, Algeria, Our products are widely recognized and trusted by users and can meet continuously developing economic and social needs. We welcome new and old customers from all walks of life to contact us for future business relationships and achieving mutual success!
  • The company keeps to the operation concept scientific management, high quality and efficiency primacy, customer supreme, we have always maintained business cooperation. Work with you,we feel easy!
    5 Stars By Dale from kazan - 2018.09.23 18:44
    In China, we have purchased many times, this time is the most successful and most satisfactory, a sincere and realiable Chinese manufacturer!
    5 Stars By Aurora from Sao Paulo - 2017.01.28 19:59
    Write your message here and send it to us